# Chamber uniformity: what ±0.5 °C means

> The two numbers on a chamber datasheet measure different things. How to read them, place sensors, and test the chamber under a real cell load.

Canonical: https://batteryxlab.com/notes/chamber-temperature-uniformity/
Language: en

- [Home](https://batteryxlab.com/)
- Resources
- [Notes](https://batteryxlab.com/notes/)
- Chamber uniformity: what ±0.5 °C means

Thermal

# Chamber uniformity: what ±0.5 °C means

The two numbers on a chamber datasheet measure different things. How to read them, place sensors, and test the chamber under a real cell load.

26 Nov 2026 · 8 min read · [All notes](https://batteryxlab.com/notes/)

A chamber datasheet usually prints two temperature numbers close together: a tight one, often ±0.5 °C, and a looser one, often ±2 °C. They are not two guesses at the same quantity. One describes how much the temperature differs between points in the chamber at a moment in time. The other describes how much a single point drifts over a period. Confusing them is one of the easiest ways to specify a chamber that looks better on paper than it behaves around a loaded cell.

The datasheets in this library make the distinction explicit in the parentheses, even where the row labels follow a different convention. This note reads those rows literally, explains what each number means for a cell, and sets out a placement and verification method that survives a real thermal load.

## Two numbers, two different questions

On the WGDW-1000-40, the performance table lists “Fluctuation ≤ ±0.5 °C (max. difference between different test points)” and “Deviation ±2 °C (max. difference of the same test point in a period of time)”. The WGDW-225-40, WGDW-408-40 and the MIHW constant-temperature chambers publish the same pair. The WGDW-380L-2-40-8CH publishes ±1 °C between test points and ±2 °C at the same point over time.

Read the parenthetical, not the label. In some laboratories “fluctuation” means the temporal variation at one point and “uniformity” means the spatial variation at one time; other vendors use the words the other way round. What matters is which measurement the number describes. For test planning, call them **spatial spread** and **temporal drift**, and record which datasheet row each came from.

| Model | Volume | Range | Spatial spread | Temporal drift |
| --- | --- | --- | --- | --- |
| WGDW-1000-40 | 1,000 L | −40 to 150 °C | ≤ ±0.5 °C between points | ±2 °C at one point over time |
| WGDW-225-40 | 225 L | −40 to 150 °C | ≤ ±0.5 °C between points | ±2 °C at one point over time |
| WGDW-380L-2-40-8CH | 380 L × 2 | −40 to 150 °C | ≤ ±1 °C between points | ±2 °C at one point over time |
| MIHW-100-2-160CH | 100 L × 2 | 0 to 60 °C | ≤ ±0.5 °C between points | ±2 °C at one point over time |

Values are from the published datasheets. The table renames the rows by what they measure; the datasheet wording is quoted in the text above.

## What ±0.5 °C does and does not tell you

Datasheet fact: the spatial number is a maximum difference between test points. It is not a statement that every point in the working volume is within ±0.5 °C of the setpoint. A chamber can have a 0.5 °C spread around a mean that is 1.5 °C away from the setpoint; the spread and the offset are different errors. The datasheet's temporal row covers drift at one point, but it does not replace a calibration of the chamber's control sensor.

The second limit is the load condition. The datasheets state the heating and cooling times as “no load, average non-linearity”, but the performance rows do not say whether the spatial and temporal numbers were measured empty or with a heat load. Do not assume they were measured with cells cycling at 1C. A chamber is a control volume with a refrigeration system, a fan and a heat-load limit; the WGDW-1000-40 publishes a heat load limit of ≤450 W. If the cells inside dissipate more than the chamber can remove at the setpoint, the air temperature will drift regardless of the empty-chamber specification.

Illustrative arithmetic: fifty cells dissipating 5 W each is 250 W, inside the published 450 W limit for the 1,000 L chamber. One hundred cells at the same 5 W is 500 W, above it. The actual heat generation depends on the cell, the current and the state of charge; the arithmetic shows why the count and the profile belong in the chamber selection, not only the volume.

## From air temperature to cell temperature

A chamber controls the air at its sensor, not the cell surface. A cell under charge has an internal temperature gradient, a tab that conducts heat to the fixture, and a surface that exchanges heat with the air at a rate set by the airflow. The cell temperature is therefore a function of the air temperature, the heat generation and the thermal resistance between the cell and the air. A ±0.5 °C air spread is a good starting condition; it is not a ±0.5 °C cell specification.

Engineering judgement: if the test result depends on cell temperature, measure the cell. Fit a thermocouple or a resistance temperature detector to a representative cell surface, and on at least one cell in the batch fit a second sensor near the tab. Compare the cell reading with the chamber reading at the same time. The difference is the offset you need to control or report. Do not apply a fixed offset from one campaign to another without checking it; the offset changes with the fixture, the airflow and the heat generation.

## Where to put the sensors

For an empty-chamber survey, use a grid that covers all three axes: top, middle and bottom; front, centre and back. Nine points is a common minimum for a small chamber; a 1,000 L chamber with a 1 m working cube benefits from more points, especially near the door, the fan outlet and the return-air path. Keep sensors away from the walls and from direct fan impingement, and shield them from radiation if the chamber walls are much hotter or colder than the air.

For a loaded survey, the grid has to follow the product. Put sensors in the tray positions that will hold cells, at the front and back of the tray, and at the top and bottom of the stack. A tray that blocks the return path can create a persistent gradient that an empty-chamber survey never sees. If the chamber has lead holes, route the sensor wires through them without leaving the door ajar; a door that does not seal changes the result.

Use a calibrated logger with a known uncertainty and a response time short enough for the test. A bare thermocouple with a fast response can read the air, but it is also sensitive to radiation; a probe with a larger thermal mass reads a mixture of air and surroundings. Record the logger model, calibration date and uncertainty with the survey. A survey reported without uncertainty cannot be compared with the datasheet.

## A survey procedure that answers the question

- **Define the operating point.** Record setpoint, ambient temperature, door state, fan setting and any humidity control. A chamber at 25 °C and a chamber at −20 °C do not have the same gradient.

- **Let the chamber stabilise.** Wait until the rate of change at every sensor is below the logger resolution over a defined interval, not for a fixed number of minutes copied from another lab.

- **Record the empty map.** Log for long enough to see the control cycle, not just one steady instant. The temporal drift is a cycle, and a short capture can miss the peak.

- **Repeat with a representative load.** Use dummy cells or the real fixture with the heat load you expect. Record the heat load in watts and the tray layout.

- **Challenge the door and the recovery.** Open the door for the time the process requires, close it, and record how long the chamber takes to return to the setpoint and to the specified spread. The datasheet notes that opening the door during a test causes temperature fluctuations; the recovery time is what the test plan needs.

- **Report the worst case.** Give the maximum spatial difference, the maximum temporal drift and the offset from setpoint, each with its uncertainty and load condition.

## What the numbers mean for a cell result

Cell voltage, impedance and self-discharge all move with temperature. A cell that sits 2 °C warmer than its neighbour is not at the same operating point, even if both are inside the chamber's published spread. The effect on a particular result has to be measured for the particular cell; it is not a universal percentage. What can be said without a cell-specific measurement is that the offset belongs in the uncertainty budget, and that comparing cells from different tray positions without recording their temperatures weakens the comparison.

For long cycle-life tests, the temporal drift matters as much as the spatial spread. If the chamber cycles around the setpoint with a ±2 °C amplitude, every cell sees the same cycle, but the cycle is part of the ageing condition. Report the chamber's control cycle and the cell-surface temperature, not only the setpoint. If the test protocol requires a tight temperature band, verify that the chamber can hold it with the load attached before the campaign starts.

## Takeaways

- The two published numbers answer different questions: ±0.5 °C is the maximum difference between test points, while ±2 °C is the drift at one point over time. Read the parenthetical, not the row label.

- The datasheet values are not a cell-temperature guarantee and do not state a load condition; verify the chamber empty and with the real heat load, and record the heat load against the published limit.

- Place sensors on a three-axis grid, add cell-surface sensors for loaded runs, and report spatial spread, temporal drift and offset from setpoint with their uncertainty.

## Request a configuration review

Tell us the channel count, current range and protocol. We will check the measurement class against the note and return a configuration, not a generic datasheet.

[Request a configuration review](https://batteryxlab.com/contact/?note=chamber-temperature-uniformity)

## References

- [WGDW-1000-40](https://batteryxlab.com/products/wgdw-1000-40-2024/) — [datasheet (PDF)](https://batteryxlab.com/assets/docs/WGDW-1000-40-2024.pdf)

- [WGDW-225-40](https://batteryxlab.com/products/wgdw-225-40/) — [datasheet (PDF)](https://batteryxlab.com/assets/docs/WGDW-225-40.pdf)

- [WGDW-380L-2-40-8CH](https://batteryxlab.com/products/wgdw-380l-2-40-8ch/) — [datasheet (PDF)](https://batteryxlab.com/assets/docs/WGDW-380L-2-40-8CH.pdf)

- [MIHW-100-2-160CH](https://batteryxlab.com/products/mihw-100-2-160ch-jade/) — [datasheet (PDF)](https://batteryxlab.com/assets/docs/MIHW-100-2-160CH-Jade.pdf)

- [WGDW series](https://batteryxlab.com/series/wgdw/)

- [MIHW series](https://batteryxlab.com/series/mihw/)

- [EV battery testing](https://batteryxlab.com/industries/ev-battery-testing/)

- [BESS testing](https://batteryxlab.com/industries/bess-testing/)

- Peer-reviewed use of this instrument class: [Temperature-dependent interphase formation and Li⁺ transport in lithium metal batteries](https://doi.org/10.1038/s41467-023-40221-0) — Weng (2023), Nature Communications. DOI: 10.1038/s41467-023-40221-0

- [Environmental chambers](https://batteryxlab.com/chambers/)

- [All datasheets](https://batteryxlab.com/resources/)

[← All technical notes](https://batteryxlab.com/notes/)

## Contact

- Email: sales@batteryxlab.com
- Phone: +852 4436 9298
- WhatsApp: https://wa.me/85244369298
- Request a quote: https://batteryxlab.com/contact/
- Full site index for agents: https://batteryxlab.com/llms.txt